Abstract
One of the principal causes of failures of transmission pipelines is volumetric metal loss due to corrosion. Various methods such as ASME B31.G, RSTRENG and the LPC methods have been developed to assess the severity of corrosion defects. The methods have developed to the extent that they are recognized by standardization bodies and regulators. However, all the methods have been developed and validated on high toughness materials. There is a concern that these methods may give non-conservative results if they are used for low toughness materials. If this is the case, guidance is required on the limits of applicability of the current methods, and new methods are required for application to low toughness materials.
To investigate these issues, contractor objectives and scope were: To test a range of representative defects in low toughness linepipe; to assess the failure mode of these defects; to determine if current assessment methods can be applied to low toughness materials; and to identify the factors influencing the failure of corrosion defects in low toughness line pipe.
Digital Access
After purchase, you will receive a download link to the report you purchased. Please confirm the email address you use to purchase the report is the email address you would like to receive the report.
If you have any trouble receiving the download instructions, please first check any spam or junk folders. Reach out to support if you need further assistance.
L51884 Assessing the Remaining Strength of Corrosion Defects in Low Toughness Linepipe Materials
Quantity
Digital products are limited to 1 per purchase
List Price
$195
Member Price
$0
Members will be redirected to a member-only report database for access to all reports. You must have a login to access reports for free.