Abstract
The welding of high strength steels in general, and for pipeline fabrication in particular, has shown that cracking due to hydrogen absorption during welding is more complex in these steels than in older, lower strength steels. In older steels, primary strengthening was accomplished with carbon, which caused hydrogen cracking in the base metal HAZ under reasonably predictable conditions involving microstructure, residual stress and hydrogen level. Pipeline steels were and are in the vanguard of change in strengthening philosophy. The change involves two areas of steel making, chemical composition and deformation processing. Pipeline steels now contain low carbon levels, in many cases <0.10%, and the resulting lack of strength is reclaimed by adding higher alloy levels to promote solution hardening (e.g. Mn), precipitation hardening (e.g. Cb, Cu) or transformation hardening (e.g. MO). In addition, alloy elements are added to improve toughness at high strength levels (e.g. Ni). At the same time, improvements have been made in reducing impurity and residual element levels, notably for S, P and O and N. Limitations on the effects of alloying additions on strength and toughness encouraged the use of deformation processing, primarily during rolling, to promote fine-grained microstructures to increase strength andtoughness simultaneously.
Electrodes for the SMAW process have been developed for welding high-strength pipeline steels by using core wires made from high-strength microalloyed skelp extruded with cellulosic (Exx10) and low hydrogen (Exx16) flux coatings. The required alloy elements for high-strength deposits were therefore obtained from the core wire and not ferroalloy powders added to the flux, as is standard industrial practice. The idea behind this change was two fold: to avoid the possibility of introducing impurities from the varying sources of ferro alloy powders, including oxygen from the oxidized powder surfaces, and also to provide a closer match of the microalloy level to modern pipeline steel chemistries. The unknowns in this work were the effects of lower impurities/similar alloy content on the mechanical properties in the cast microstructure of a weld, compared to a pipe, and of the effect on electrode welding behaviour of a flux containing no ferro powders other than FeSi.
Digital Access
After purchase, you will receive a download link to the report you purchased. Please confirm the email address you use to purchase the report is the email address you would like to receive the report.
If you have any trouble receiving the download instructions, please first check any spam or junk folders. Reach out to support if you need further assistance.
L51706 Higher-Strength SMAW Filler Metals
Quantity
Digital products are limited to 1 per purchase
List Price
$249
Member Price
$0
Members will be redirected to a member-only report database for access to all reports. You must have a login to access reports for free.