Research Report Library > Reports
Report
L51674 In-Line Inspection Device for Stress Corrosion Cracks
Abstract
 Under previous programs for the Pipeline Research Committee, field tested a low frequency eddy current instrument for detecting and characterizing stress corrosion cracks in pipelines was developed. While a significant improvement over conventional magnetic particle inspections in some respects, the eddy current method as it was developed in these programs can only be used with surface breaking defects. Thus, it is limited to use for inspections of pipelines from the outside surface.
In this program, we examined the use of a saturating magnetic field to allow increased penetration of the eddy current field into the pipe material, providing the ability to detect and characterize stress corrosion cracks from the interior of the pipeline. Until recently, eddy current inspections of steel were the exception not the norm, primarily because low frequency eddy current instruments were not available. In eddy current testing, the eddy current field grows smaller as it penetrates into the material being tested.
Digital Access
After purchase, you will receive a download link to the report you purchased. Please confirm the email address you use to purchase the report is the email address you would like to receive the report.
If you have any trouble receiving the download instructions, please first check any spam or junk folders. Reach out to support if you need further assistance.
L51674 In-Line Inspection Device for Stress Corrosion Cracks
Quantity
Digital products are limited to 1 per purchase
List Price
$395
Member Price
$0
Members will be redirected to a member-only report database for access to all reports. You must have a login to access reports for free.