Abstract
A large amount of inspection data was generated from the inspection of 36 weld defects included in Phases I and II of PRCI Project number PR-166-177. For convenience of reporting and because most readers till not require it, this data was largely left out of the final report. However, because the data generated may be of interest to some and because it is likely to have direct relevance to projects planned for the future it was considered expedient to formally record this data. Results are reported in two sections. Section 1 containing results from Phase I and Section 2 the results from Phase II. All information including inspector’s comments, multiple A-scans and photographs of exposed defects (where available) are included for each defect under its own sub section. Describes experimental work to investigate the use of focused ultrasonic beams for sizing girth weld defects in large diameter pipe. Transducer and lens design are discussed. A comparison of results of destructive examinations is given.
Digital Access
After purchase, you will receive a download link to the report you purchased. Please confirm the email address you use to purchase the report is the email address you would like to receive the report.
If you have any trouble receiving the download instructions, please first check any spam or junk folders. Reach out to support if you need further assistance.
L51493 Sizing of Girth Weld Defects Using Focused Ultrasonic Beams Phases I and II
Quantity
Digital products are limited to 1 per purchase
List Price
$195
Member Price
$0
Members will be redirected to a member-only report database for access to all reports. You must have a login to access reports for free.